DOI:  10.1016/j.corsci.2016.12.012  Effects of microtexture and Ti3Al (α2) precipitates on stress-corrosion cracking properties of a Ti-8Al-1Mo-1V alloy
Author: Cao, Sheng.  v. 116  pp. 22- 33  Date: 2017